斷裂伸長率 | 600% | 拉伸強度 | 15MPa | 密度 | 0.92g/cm3 |
熔體流動速率 | 1g/10min | 維卡軟化點 | 102℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
|
產品簡述
斷裂伸長率 | 600% | 拉伸強度 | 15MPa | 密度 | 0.92g/cm3 |
熔體流動速率 | 1g/10min | 維卡軟化點 | 102℃ | 用途級別 | 薄膜級 |
規(guī)格級別 | 薄膜 |
詳細數(shù)據
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據 | 數(shù)據單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.920 | g/cm3 | ||
機械性能 | 斷裂抗張強度 | MD | ASTM D-882 | 220 | kg/cm2 | |
TD | ASTM D-882 | 160 | kg/cm2 | |||
抗沖擊強度 | ASTM D-1709 | 240 | g/F50 | |||
降伏點抗張強度 | MD | ASTM D-882 | 100 | kg/cm2 | ||
TD | ASTM D-882 | 90 | kg/cm2 | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 102 | ℃ | ||
其它性能 | 伸長率 | ASTM D-882 | 500 | % | ||
光澤度 | ASTM D-523 | 110 | % | |||
霧度 | ASTM D-1003 | 14 | % | |||
熔融指數(shù) | ASTM D-1238 | 1.0 | g/10min | |||
收縮率 | ASTM D-995 | 2 | % | |||
低溫脆裂溫度 | ASTM D-746 | <-76 | ℃ | |||
熔點 | ASTM D-2117 | 122 | ℃ | |||
伸長率 | ASTM D-882 | 600 | % |