斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 36MPa | 密度 | 0.919g/cm3 |
熔體流動(dòng)速率 | 2.1g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
缺口沖擊強(qiáng)度 | 6 |
|
產(chǎn)品簡述
斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 36MPa | 密度 | 0.919g/cm3 |
熔體流動(dòng)速率 | 2.1g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
缺口沖擊強(qiáng)度 | 6 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
熔體流動(dòng)速率 | ASTM D-1238 | 2.1 | g/10min | |||
機(jī)械性能 | 抗沖擊強(qiáng)度 | ASTM D-3420 | 6 | Kg/cm | ||
伸長率 | MD | ASTM D-882 | 700 | % | ||
TD | ASTM D-882 | 750 | % | |||
撕裂強(qiáng)度 | MD | ASTM D-1922 | 10 | g/µm | ||
TD | ASTM D-1922 | 12 | g/µm | |||
拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 100 | Kg/cm2 | ||
TD | ASTM D-882 | 100 | Kg/cm2 | |||
拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 410 | Kg/cm2 | ||
TD | ASTM D-882 | 370 | Kg/cm2 | |||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 102 | ℃ | ||
脆化溫度 | ASTM D-746 | <-70 | ℃ | |||
其它性能 | 薄膜厚度 | ASTM D-746 | 30 | µm | ||
霧度 | ASTM D-1003 | 2 | % |