斷裂伸長(zhǎng)率 | 800% | 拉伸強(qiáng)度 | 46MPa | 密度 | 0.919g/cm3 |
熔體流動(dòng)速率 | 1g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
缺口沖擊強(qiáng)度 | 12 |
|
產(chǎn)品簡(jiǎn)述
斷裂伸長(zhǎng)率 | 800% | 拉伸強(qiáng)度 | 46MPa | 密度 | 0.919g/cm3 |
熔體流動(dòng)速率 | 1g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
缺口沖擊強(qiáng)度 | 12 |
詳細(xì)數(shù)據(jù)
訂購(gòu)指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 1 | g/10min | ||
密度 | ASTM D-1505 | 0.919 | g/cm3 | |||
機(jī)械性能 | 拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 120 | Kg/cm2 | |
TD | ASTM D-882 | 110 | Kg/cm2 | |||
抗沖擊強(qiáng)度 | ASTM D-3420 | 12 | Kg/cm | |||
伸長(zhǎng)率 | MD | ASTM D-882 | 700 | % | ||
TD | ASTM D-882 | 800 | % | |||
拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 520 | Kg/cm2 | ||
TD | ASTM D-882 | 470 | Kg/cm2 | |||
撕裂彈性率 | MD | ASTM D-882 | 2200 | Kg/cm2 | ||
TD | ASTM D-882 | 2700 | Kg/cm2 | |||
撕裂強(qiáng)度 | MD | ASTM D-1004 | 12 | Kg/cm | ||
TD | ASTM D-1004 | 18 | Kg/cm | |||
熱性能 | 脆化溫度 | ASTM D-746 | <-80 | ℃ | ||
維卡軟化點(diǎn) | ASTM D-1525 | 102 | ℃ | |||
其它性能 | 薄膜厚度 | ASTM D-746 | 50 | µm | ||
霧度 | ASTM D-1003 | 9 | % |