斷裂伸長率 | 800% | 拉伸強度 | 52MPa | 密度 | 0.928g/cm3 |
熔體流動速率 | 1g/10min | 維卡軟化點 | 105℃ | 用途級別 | 薄膜級,纖維 |
規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
產(chǎn)品簡述
斷裂伸長率 | 800% | 拉伸強度 | 52MPa | 密度 | 0.928g/cm3 |
熔體流動速率 | 1g/10min | 維卡軟化點 | 105℃ | 用途級別 | 薄膜級,纖維 |
規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.928 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 1 | g/10min | |||
機械性能 | 拉伸屈服強度 | MD | ASTM D-882 | 165 | Kg/cm2 | |
TD | ASTM D-882 | 150 | Kg/cm2 | |||
拉伸斷裂強度 | MD | ASTM D-882 | 590 | Kg/cm2 | ||
TD | ASTM D-882 | 530 | Kg/cm2 | |||
伸長率 | MD | ASTM D-882 | 700 | % | ||
TD | ASTM D-882 | 800 | % | |||
撕裂強度 | MD | ASTM D-1922 | 10 | g/µm | ||
TD | ASTM D-1922 | 15 | g/µm | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 105 | ℃ | ||
脆化溫度 | ASTM D-746 | <-80 | ℃ | |||
其它性能 | 薄膜厚度 | ASTM D-746 | 50 | µm |