用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 | 加工級別 | 吹塑級,擠出級 |
|
產(chǎn)品簡述
用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 | 加工級別 | 吹塑級,擠出級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 熔體流動速率 | ASTM D-1238 | 0.45 | g/10min | ||
密度 | ASTM D-1505 | 0.921 | g/cm3 | |||
物理性能 | 霧度 | ASTM D-1003 | 9.0 | % | ||
光澤度 | 45℃ | ASTM D-2457 | 70 | |||
薄膜厚度 | HYUNDAI | 60 | μm | |||
機械性能 | 斷裂伸長率 | ASTM D-638 | 600 | % | ||
屈服拉伸強度 | ASTM D-638 | 93 | Kg/cm2 | |||
落球沖擊強度 | ASTM D-1709 | 180 | g | |||
斷裂伸長率 | MD | ASTM D-882 | 350 | % | ||
TD | ASTM D-882 | 550 | % | |||
斷裂拉伸強度 | MD | ASTM D-882 | 280 | kg/cm2 | ||
TD | ASTM D-882 | 260 | kg/cm2 | |||
斷裂拉伸強度 | ASTM D-638 | 160 | Kg/cm2 | |||
肖氏硬度 | ASTM D-2240 | 52 | D SCALE | |||
伸長彈性率 | ASTM D-638 | 1200 | Kg/cm2 | |||
熱性能 | 熔點 | HPC | 105 | ℃ | ||
維卡軟化點 | ASTM D-1525 | 94 | ℃ |