| 斷裂伸長率 | 620% | 拉伸強度 | 21.5MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 0.7g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
| 缺口沖擊強度 | 130 |
|
|
產品簡述
| 斷裂伸長率 | 620% | 拉伸強度 | 21.5MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 0.7g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
| 缺口沖擊強度 | 130 |
詳細數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-792 | 0.924 | g/cm3 | ||
| 熔體流動速率 | 190℃/2.16kg | ASTM D-1238 | 0.70 | g/10min | ||
| 機械性能 | 屈服拉伸強度 | MD | ASTM D-882 | 10.5 | MPa | |
| TD | ASTM D-882 | 11.0 | MPa | |||
| 斷裂拉伸強度 | MD | ASTM D-882 | 25.4 | MPa | ||
| TD | ASTM D-882 | 21.5 | MPa | |||
| 斷裂伸長率 | MD | ASTM D-882 | 330 | % | ||
| TD | ASTM D-882 | 620 | % | |||
| 沖擊強度 | ASTM D-1709 | 130 | g | |||
| 埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 270 | g | ||
| TD | ASTM D-1922 | 190 | g | |||
| 其它性能 | 薄膜厚度 | 38.1 | μ | |||
| 薄膜硬度 | MD | ASTM D-882 | 66.4 | J/CM3 | ||
| TD | ASTM D-882 | 79.0 | J/CM3 | |||
| 光學性能 | 光澤度 | 45° | ASTM D-2457 | 55 | ||
| 霧度 | ASTM D-1003 | 9.9 | % | |||