| 斷裂伸長率 | 610% | 拉伸強度 | 49MPa | 密度 | 0.952g/cm3 |
| 熔體流動速率 | 0.15g/10min | 維卡軟化點 | 125℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 610% | 拉伸強度 | 49MPa | 密度 | 0.952g/cm3 |
| 熔體流動速率 | 0.15g/10min | 維卡軟化點 | 125℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
詳細數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.952 | g/cm3 | ||
| 熔體流動速率 | ASTM D-1238 | 0.15 | g/10min | |||
| HLMI | ASTM D-1238 | 16 | g/10min | |||
| 機械性能 | 1%割線模量 | MD | ASTM D-882 | 1400 | MPa | |
| TD | ASTM D-882 | 1700 | MPa | |||
| 斷裂拉伸強度 | MD | ASTM D-882 | 55 | MPa | ||
| TD | ASTM D-882 | 49 | MPa | |||
| 斷裂伸長率 | MD | ASTM D-882 | 400 | MPa | ||
| TD | ASTM D-882 | 610 | MPa | |||
| 屈服拉伸強度 | MD | ASTM D-1505 | 31 | MPa | ||
| TD | ASTM D-1505 | 30 | MPa | |||
| Elmendorf斷裂強度 | MD | ASTM D-1922 | 4 | g | ||
| TD | ASTM D-1922 | 40 | g | |||
| Dart沖擊強度 | F50 | ASTM D-1709 | 180 | g | ||
| 熱性能 | 維卡軟化點 | ASTM D-1525 | 125 | ℃ | ||