| 密度 | 0.938g/cm3 | 熔體流動(dòng)速率 | 19g/10min | 維卡軟化點(diǎn) | 60℃ |
| 硬度 | 34 | 規(guī)格級(jí)別 | 注塑 | 脆化溫度 | -76℃ |
| 加工級(jí)別 | 注塑級(jí),熱熔級(jí) |
|
|
產(chǎn)品簡(jiǎn)述
| 密度 | 0.938g/cm3 | 熔體流動(dòng)速率 | 19g/10min | 維卡軟化點(diǎn) | 60℃ |
| 硬度 | 34 | 規(guī)格級(jí)別 | 注塑 | 脆化溫度 | -76℃ |
| 加工級(jí)別 | 注塑級(jí),熱熔級(jí) |
詳細(xì)數(shù)據(jù)
訂購(gòu)指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.938 | g/cm3 | ||
| 其它性能 | 鑄膜成型 | ASTM D-638/D-882 | 790 | % | ||
| 融化點(diǎn) | ASTM D-2117 | 82 | ℃ | |||
| 熔融指數(shù) | ASTM D-1238 | 19 | g/10min | |||
| 薄膜 | MD | ASTM D-638/D-882 | 138 | kg/cm2 | ||
| TD | ASTM D-638/D-882 | 86 | kg/cm2 | |||
| 射出 | ASTM D-638/D-882 | 300 | % | |||
| VA含量 | ASTM USIFE | 20 | % | |||
| 薄膜 | MD | ASTM D-638/D-882 | 450 | % | ||
| TD | ASTM D-638/D-882 | 660 | % | |||
| 硬度 | ASTM D-2240 | 34 | Shore D | |||
| 鑄膜成型 | ASTM D-638 | 127 | kg/cm2 | |||
| 低溫易脆性 | ASTM D-746 | <-76 | ℃/F50 | |||
| VICAT 軟化點(diǎn) | ASTM D-1525 | 60 | ℃ | |||
| 射出 | ASTM D-638/D-882 | 72 | kg/cm2 | |||